Shandong Weichuan Metal Prodducts Co., Ltd.

4135 34crmo4 35CD4 alloy steel pipe manufacturer spot warranty sales

Short Description:

ASTM 4135 has high static strength, impact toughness and higher fatigue limit, higher hardenability than 40Cr, high creep strength and endurance strength at high temperature, long-term working temperature up to 500℃; plasticity during cold deformation Medium, poor weldability.
Foreign name ASTM 4135 alloy structural steel 4135
Alloy structural steel: 4135
Executive standard: ASTM A29/A29M-04
●Characteristics and scope of application:
It has high static strength, impact toughness and higher fatigue limit, higher hardenability than 40Cr, high creep strength and endurance strength at high temperature, long-term working temperature up to 500℃; medium plasticity during cold deformation, Poor weldability. Used as important structural parts that work under high loads, such as transmission parts of vehicles and engines; rotors, main shafts, heavy-load transmission shafts of steam turbine generators, and large-section parts.
●Chemical composition:
Carbon C: 0.33~0.38
Silicon Si: 0.15~0.35
Manganese Mn: 0.70~0.90
Sulfur S: allowable residual content ≤0.040
Phosphorus P: allowable residual content ≤0.035
Chromium Cr: 0.80~1.10
Nickel Ni: allowable residual content ≤0.030
Copper Cu: allowable residual content ≤0.030
Molybdenum Mo: 0.15~0.25
●Mechanical properties:
Tensile strength σb (MPa): ≥985(100)
Yield strength σs (MPa): ≥835(85)
Elongation δ5 (%): ≥12
Reduction of area ψ (%): ≥45
Impact energy Akv (J): ≥63
Impact toughness value αkv (J/cm2): ≥78(8)
Hardness: ≤229HB
Sample size: sample blank size is 25mm
●Heat treatment specifications and metallographic structure:
Heat treatment specification: quenching 850℃, oil cooling; tempering 550℃, water cooling, oil cooling.
●Delivery status: delivery with heat treatment (normalizing, annealing or high temperature tempering) or without heat treatment. The delivery status should be indicated in the contract. [1-2]
●Corresponding national brands:
Corresponding domestic grades: 35CrMo
Corresponding Japanese brand: SCM435 (SCM3)
Corresponding to German brand: 34CrMo4(1.7220)
Corresponding British grades: 708A37
Corresponding French brand: 35CD4


Product Detail

Product Tags

Description

35CrMo is the specification number of alloy structural steel (alloy quenched and tempered steel), which is mainly used to manufacture important parts in various machines bearing impact, bending and torsion and high load. The unified digital code of 35CrMo alloy structural steel (alloy quenched and tempered steel) is a30352, and the executive standard is GB / t3077-2015

35crmo

35CrMo (2 sheets)

Italy: 35crmo4

NBN: 34crmo4

Sweden: 2234

Daily standard: scm432 / sccrm3

35CrMo alloy steel pipe manufacturer spot warranty sales

It is used to manufacture important parts in various machines bearing impact, bending and torsion and high load, such as herringbone gear, crankshaft, hammer rod, connecting rod and fasteners of steel rolling mill, main shaft and axle of steam turbine engine, engine transmission parts, large motor shaft, perforator in petroleum machinery, boiler bolts with working temperature lower than 400 ℃, nuts with working temperature lower than 510 ℃, High pressure seamless thick wall conduit (temperature 450 ~ 500 ℃, no corrosive medium) in chemical machinery; It can also replace 40crni for manufacturing high load transmission shaft, steam turbine engine rotor, large section gear, support shaft (diameter less than 500mm), etc; Process equipment materials, pipes, welding materials, etc.

Used as important structural parts working under high load, such as transmission parts of vehicles and engines; Rotor, main shaft, heavy load transmission shaft and large section parts of steam turbine generator.

Chemical composition

Carbon C: 0.32 ~ 0.40

Silicon Si: 0.17 ~ 0.37

Mn: 0.40 ~ 0.70

Sulfur s: allowable residual content ≤ 0.035

Phosphorus P: allowable residual content ≤ 0.035

Cr: 0.80 ~ 1.10

Nickel: allowable residual content ≤ 0.30

Copper Cu: allowable residual content ≤ 0.30

Mo: 0.15 ~ 0.25

Mechanical property

Tensile strength σ b (MPa): ≥985(100)

Yield strength σ s (MPa): ≥835(85)

Elongation δ 5 (%): ≥12

Reduction of area ψ (%):  ≥45

Impact energy Akv (J): ≥ 63

Impact toughness value α kv (J/cm²):  ≥78(8)

Hardness: ≤ 229hb

Sample size: sample blank size is 25mm

Heat treatment specification and metallographic structure

Heat treatment specification: quenching 850 ℃, oil cooling; Tempering 550 ℃, water cooling, oil cooling.

Mechanical properties

Steel grade: 35CrMo

Sample blank size / mm: 25

Heat treatment | quenching | heating temperature / ℃ | first quenching: 850

Heat treatment | quenching | heating temperature / ℃ | second quenching: --

Heat treatment | quenching | coolant: Oil

Heat treatment | tempering | heating temperature / ℃: 550

Heat treatment | tempering | coolant: water, oil

Mechanical properties | tensile strength σ b/MPa|≥: 980

Mechanical properties | yield point σ s/MPa|≥: 835

Mechanical properties | elongation δ 5(%)|≥: 12

Mechanical properties | surface shrinkage ψ(%)| ≥: 45

Mechanical properties | impact absorption energy Akv / J | ≥: 63

Delivery state hardness HBS | ≥: 229

Delivery status: delivery in heat treatment (normalizing, annealing or high temperature tempering) or non heat treatment status, and the delivery status shall be indicated in the contract.


  • Previous:
  • Next:

  • Related Products